產品詳情
編號:1.4749
分類:鐵素體耐熱鋼
密度:7.7 g/cm3
標準:
EN 10095:1999耐熱鋼和鎳合金
EN 10297-2:2005機械和一般工程用無縫圓形鋼管。不銹鋼。技術交付條件
EN 10088-1:2005不銹鋼。不銹鋼清單
Chemical comb % of steel X15CrN26 EN 10095-1999
| C | Si | Mn | P | S | Cr | N |
| 0.15 - 0.2 | max 1 | max 1 | max 0.04 | max 0.015 | 26 - 29 | 0.15 - 0.25 |
Rm - Tensile strength (MPa) (+A) 500-700
Rp0.2 0.2% proof strength (MPa) (+A) 280
A - Min. elongation at fracture (%) (+A) 13-15
Brinell hardness (HB): (+A) 212
Properties of steel X15CrN26
Maximum application temperature for air T= 1100 ° C
Equivalent grades of steel X15CrN26 Warning! Only for reference
EU USA Inter
EN - ISO
X18CrN28 446 X15CrN26
S44600